MEMSnet Home: MEMS-Talk: Silicon and germanium defect delineation
Silicon and germanium defect delineation
2006-06-26
Andrea Mazzolari
2006-06-27
Kirt Williams
Silicon and germanium defect delineation
Andrea Mazzolari
2006-06-26
Hi all.
When dicing a silicon wafer, near the diced surface are produced defects
and, i think, silicon become amorphous. Thickness of damaged layer is
function of blade grit and dicing speed. Is there a way to delineate this
type of defects?
Could silicon defects delineation etches help? Can someone suggest me some
articles about silicon defects delineation etches?

For completely different tasks i'm interested also to germanium defects
delineation etches. Could someone suggest me articles?

Sorry for bad english,
thanks
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer