A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to fabricate rounded channels
How to fabricate rounded channels
2006-06-26
t yt
2006-06-26
Li Wang
2006-06-26
Joseph Grogan
2006-06-26
Jaephil Do
2006-06-27
t yt
2006-06-27
Ching-Lung Chen [陳慶隆]
2006-06-26
Lung-hao Hu
2006-06-27
Lung-hao Hu
How to fabricate rounded channels
Jaephil Do
2006-06-26
You may try a photoresist reflow technique.
First pattern photoresist and reflow in a heated oven
This technique has been used to make microlense.

Jaephil Do, Graduate Research Assistant
Microsystems and BioMEMS Lab. Rhodes hall #919
Dept. of ECECS, University of Cincinnati
Cincinnati, OH 45221-0030
Phone: (513) 556-0852, Fax: (513) 556-7326
eMail: [email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Joseph Grogan
Sent: Monday, June 26, 2006 12:40 PM
To: General MEMS discussion
Subject: Re: [mems-talk] How to fabricate rounded channels

Ho big does your channel need to be?
-Joe Grogan

t yt wrote:
> Hi all,
>
>   I want to fabricate a rounded channel from PDMS. Still i have no idea
about how to fabricate a rounded mold. Is there anyone who can give me
suggestion?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review