A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to fabricate rounded channels
How to fabricate rounded channels
2006-06-26
t yt
2006-06-26
Li Wang
2006-06-26
Joseph Grogan
2006-06-26
Jaephil Do
2006-06-27
t yt
2006-06-27
Ching-Lung Chen [陳慶隆]
2006-06-26
Lung-hao Hu
2006-06-27
Lung-hao Hu
How to fabricate rounded channels
t yt
2006-06-27
Hi Grogan,

  The channel should have the width of 5 mm, and the depth of approximately 30
um.

  Thanks!



Joseph Grogan  wrote:
  Ho big does your channel need to be?
-Joe Grogan

t yt wrote:
> Hi all,
>
> I want to fabricate a rounded channel from PDMS. Still i have no idea about
how to fabricate a rounded mold. Is there anyone who can give me suggestion?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing