kris
2006-06-30
Rajib Ahmed
2006-06-30
Bill Moffat
2006-06-30
PRAMOD GUPTA
Planar deposition of PI 2610
Rajib Ahmed
2006-06-30
Maybe you can try dip coating.  Once you take the sample out of the parent
solution, you can use a doctor blade to wipe off the excess and have a
uniform thickness of 1 micron.  They make different thicknesses of doctor
blades that give you a wide range.  This process, if I recall correctly,
is known as "knife coating."  So you would have to do a 2-step process,
start with dip coating to fill up the trenches and then do a knife coating
to attain teh required surface coverage thickness.

*******************************************************************************
Rajib Ahmed
347 Hopeman Engineering Building
Department of Electrical and Computer Engineering
University of Rochester
Rochester, NY 14627-0167
Email:[email protected]
Phone#:(585)275-8093
Fax#:(585)273-4919
*******************************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.
The Branford Group