I want to do DC sputtering of Chromium (as an adhesive layer) and
platinum (as an electrode layer on soda lime glass. Do i need to do
any surface treatment of glass apart from cleaning? Can someone tell
me the deposition rate of platinum if argon gas is used in sputtering
and what is the pressure of Argon required for that.

it would be very helpful if someone suggest me a reference paper for
DC sputtering of metal on glass.
--
RUPESH SAWANT
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.
Tanner EDA by Mentor Graphics