shay kaplan
2006-07-08
walter essinger
Ion Mill Services
walter essinger
2006-07-08
Not knowing the details I am asuming that you have a 1 micon thick Pt layer
which you need to pattern.
If all fails may I suggest a lift of process works well with Pt and saves
money.
Regards
Walter
[email protected]
----- Original Message -----
From: "Phillipe Tabada" 
To: 
Sent: Friday, July 07, 2006 11:44 AM
Subject: [mems-talk] Ion Mill Services


> Hi,
>
>  Looking for a company who can ion mill 1 um of Pt using photoresist as
> a mask.  Then remove the mask using wet etching (no ashing).  This is for
> low volume research quantities.
>
> Phil
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics