Hi Nels,

> Here is one that I used for crystalline germanium:
> R. Leancu, N. Moldovan, L. Csepregi, and W. Lang, "Anisotropic etching of
> germanium," Sensors and Actuators A, vols. 46-47, pp. 35-37, 1995.

can you give me more informations?
Which type of wafer have you used ? (100) like in the article you suggested
me ?
Which mask have you used ? A Cr mask like suggested in this article or
another type of mask?
Which etchant? It seams article suggest ellison or kern solutions. Do you
know etch rate of those solutions? They are not reported in the article :OO

Do you have any informations about isotropic etching of germanium ? In
particular, reading the article you suggested, it seams that Billing and
Holmes solutions are isotropic etchants, is this correct ?

> I am pretty sure that these same authors also published another paper on
> the topic in another journal but I cannot find it at this time.

I've found this
Synchrotron-radiation-induced wet etching of germanium,  Applied Physics
Letters -- August 26, 2002 -- Volume 81, Issue 9, pp. 1741-1743
Bulk micromachining of Ge for IR gratings
W Lang et al 1996 J. Micromech. Microeng. 6 46-48

Does someone have informations also about isotropic etching of germanium ?

Thanks
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group