MEMSnet Home: MEMS-Talk: Micromachining (Removing) Dominant Pyramid Features in Quartz
Micromachining (Removing) Dominant Pyramid Features in Quartz
2006-07-14
Ron Martin
Micromachining (Removing) Dominant Pyramid Features in Quartz
Ron Martin
2006-07-14
        We make a device where we do a step etch on a part of the device to
thin out that specific feature (thin it out for dampening).  We use HF to
perform the etch.  However, we form unwanted dominant pyramid features (due
to contamination and surface defects at the starting quartz plane) by the
time we end the etch.  Has anyone have any experience with removing these
unwanted features using laser micromachining (or any other method)?  Our
concern with this method would be its potential damage to the device
structure (micro fractures) as a result of forced ablation.  The pyramid
dimension are typically 40 um or higher, and 120 um wide or greater in the
base.

Ron Martin

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group
Nano-Master, Inc.