MEMSnet Home: MEMS-Talk: remove barrier layer
remove barrier layer
2006-07-18
B.Frank
remove barrier layer
B.Frank
2006-07-18
Hi, friends,
Is there anybody who has experinece on making anodic aluminum oxide(AAO)?
I want to transfer the pattern of the AAO to silicon dioxide using dry etching,
so i need to remove the barrier layer at the bottom. I tried several methods
such as 30degreeC H3PO4 20min. But it didn't work.

Another question is how to clean the film after strip off from the film. I use
HgCl2 to strip the AAO film from the film, but it is dirt. It is difficult to
clean up. is there anybody has any experience?
Thank you. Have a good day.

University of California,Irvine
B.Frank
[email protected]
2006-07-18

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMStaff Inc.
Mentor Graphics Corporation