Hi, everyone,
Is there anyone has recipe to planar etch silicon?
I want to etch silicon wafer to make a mesa about 500~1000nm height.
The doping concentration is varing from 10^18 to 10^16. So I want a
non-doping related recipe. Is there rated information for the etching
rate?
Thank you very much.