I was wondering if anyone has experience with anisotropic RIE of glass.
I would like to form straight walled channels in microscope slides
(sodalime) or coverslips (zinc titania). I found some papers on the
topic but didn't have much success with their suggestions so I was
hoping to find someone with personal experience.

thanks in advance for any responses.

-Joe Grogan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics