anisotropic etching of glass
2006-08-01
Joe Grogan
2006-08-02
Brent Garber
anisotropic etching of glass
Brent Garber
2006-08-02
Joe,

Have you tried SF6, 75 watts, with a chamber pressure less than 10 mT?
Every RIE acts differently.

Brent

Joe Grogan wrote:

> Hi all,
>
> I was wondering if anyone has experience with anisotropic RIE of glass.
> I would like to form straight walled channels in microscope slides
> (sodalime) or coverslips (zinc titania). I found some papers on the
> topic but didn't have much success with their suggestions so I was
> hoping to find someone with personal experience.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review