PRS 3000 & aluminum
2006-08-04
Andreas K. Huettel
PRS 3000 & aluminum
Andreas K. Huettel
2006-08-04
Dear all,

I've heard rumors that PRS-3000 photoresist stripper does not go well with
aluminum (nano-)structures.

Does anyone know any details on this?

Best,  Andreas Huettel

- ---------------------------------------------------------------------
Dr. Andreas K. Huettel                  tel. +31 15 27 88102  (univ.)
Molecular Electronics and Devices            +31 6 42527466  (mobile)
Kavli Institute of Nanoscience Delft    [email protected]
Delft University of Technology             [email protected]
PO Box 5046, 2600 GA Delft                          [email protected]
The Netherlands                     http://www.akhuettel.de/research/
- ---------------------------------------------------------------------
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Addison Engineering
University Wafer