Hi,
For increasing CF4 flow, can anyone indicate to me what the general
etchrate uniformity
trend would be for Epi Silicon exposed to a plasma
fluoro carbon chemistry of CHF3/CF4 at >500W, at
medium pressure?

Thank you for the consideration.

Philip