I've heard the HMDS works well as a mold release for PDMS.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Z xy
Sent: Tuesday, August 15, 2006 11:57 AM
To: [email protected]
Subject: [mems-talk] Release agent(PDMS-Silicon)

Hi,
We are looking for a type of mold release agent used for stripping off
the PDMS layer from the silicon mold in nanoimprint fab. We basically
want to make it much easier to strip off the thermal cured PDMS layer
from the nanopatterned silicon template. Can anyone tell us where to buy
such release agent or if there is any other solutions?
Rayne


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing