A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: 10 nanometer hole
10 nanometer hole
2006-08-17
[email protected]
2006-08-17
Roger Shile
2006-08-18
Isaac Chan
2006-08-19
Jacques Jonsmann
2006-08-20
Jeehwan Kim
2006-08-22
Glenn Silveira
2006-08-21
Glenn Silveira
Re: 10 nanometer hole
2006-08-18
mohendra roy
2006-08-21
Jim Beall
2006-08-19
[email protected]
2006-08-21
[email protected]
2006-08-21
Rob Knobel
2006-08-21
[email protected]
Re: 10 nanometer hole
mohendra roy
2006-08-18
First tell me what is your film type. if it is polymer you can make
your desired hole by ion irradiation.

On 17/08/06, [email protected]  wrote:
> Does anyone know how and who can make a 10 nanometer hole in a 50 nanometer
> film.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics