Subject: [mems-talk] Etching TiAlN
2006-08-22
Jeff Kettle
Subject: [mems-talk] Etching TiAlN
Jeff Kettle
2006-08-22
  Hi,

I know we have used in the past Inductively coupled Plasma (ICP) RIE for etching
of TiAlN, the main problem with this is that the etch rate is typically very
slow (5-7nm/min). However, can generate very isotropic etched structures (gate
electrodes as well in this case) and the slowness allows for good control of
etch depth.

  Regards,

  Jeff Kettle

  Forwarded Message

From:  "Vikram"     To:  [email protected]    Date:
Tue, 22 Aug 2006 04:32:19 -0700 (PDT)    Subject:  [mems-talk] Etching TiAlN

Hi Friends,      Could anyone tell me how to etch TiAlN layer over a silicon-di-
oxide   layer? I am working on gate electrodes for MOSFET. Any other ideas to
use other matals for the same are wlecome.     Regards  Vikram
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation