VCSEL excites the photoluminescence
2006-08-29
Lung-hao Hu
VCSEL excites the photoluminescence
Lung-hao Hu
2006-08-29
Hi

Is there any VCSEL whose power is high enough to exicte the photoluminescence ??
My sample is SiCNO derived from Ceraset polymer (PUMV).

Best regards,

Lung-hao Hu

Graduate Student

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
UCB 427 CO 80309 U.S.A
Email:[email protected]
Tel:303-786-1702(H)
    303-492-6107(O)
Fax:303-492-3498
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.