MEMSnet Home: MEMS-Talk: Regarding Glass lithography
Regarding Glass lithography
2006-08-29
Kannan Ramaraj
2006-08-29
Gareth Jenkins
2006-08-30
Marc Häfner
Re: AW: [mems-talk] Regarding Glass lithography
2006-08-30
sokwon Paik
2006-09-01
walter essinger
2006-09-01
Xiaoguang "Leo" Liu
2006-09-03
walter essinger
2006-08-29
Bill Moffat
2006-08-30
Gareth Jenkins
2006-08-31
Kirt Williams
Regarding Glass lithography
Marc Häfner
2006-08-30
Hi,

you can also use Titanium as adhesion layer....

Regards

Marc

-----Ursprüngliche Nachricht-----
Von: Kannan Ramaraj [mailto:aerokannan@rediffmail.com]
Gesendet: Dienstag, 29. August 2006 12:51
An: mems-talk@memsnet.org
Betreff: [mems-talk] Regarding Glass lithography


Hi all!
    I am trying to make one-dimensional groove pattern over the glass
surface with a width and depth ranging from 50micron to 200 micron. I
laminated dry photoresist over the glass surface and prepared the pattern in
the glass surface. Photoresist is not staying more than 1 minute if i put it
in dilute HF. And also I read in this site that I can use Chromium as a
sacrificial layer. But I don't have chromium with me. Can you suggest some
other material as a sacrificial layer ? Whether I have to coat my
sacrificial layer before or after the photoresist ? Please give some idea to
overcome this issue.
          Thanks!
                                  With regards,
                                    R.Kannan


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing