MEMSnet Home: MEMS-Talk: dissolving cured epoxy glue
dissolving cured epoxy glue
2006-09-04
Mohammad Najmzadeh
2006-09-05
ssood
2006-09-05
Mohammad Najmzadeh
2006-09-04
[email protected]
dissolving cured epoxy glue
Mohammad Najmzadeh
2006-09-04
Hello,

I have attached some silicon sensors to an aluminium setup with epoxy glue
and now I want to disconnect them.

I am looking for a way to dissolve this cured epoxy glue.

Heating of it for 3 hours on a hot plate with 200-300 degree C was one
option to dissociate that glue but that was not successful.

Please inform me if you know anything about it.

Kind Regards,
Mohammad Najmzadeh

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.