Adhesive layer for gold on oxide and patterning
2006-09-08
J.J HU
2006-09-08
walter essinger
2006-09-12
Kirt Williams
Adhesive layer for gold on oxide and patterning
walter essinger
2006-09-08
Greetings,
Ti,Cr etc yes lift- off is the best option
regards
[email protected]
----- Original Message -----
From: "J.J HU" 
To: 
Sent: Friday, September 08, 2006 8:09 AM
Subject: [mems-talk] Adhesive layer for gold on oxide and patterning


> Hi all,
> I am trying to put down 300~500nm Au film on Si dioxide as electrodes, and
> I
> am just wondering what kind of adhesive layer (needs to be electrically
> conductive) should I deposit before Au to improve the adhesion?
>
> And anyone has some good thoughts about how to pattern the gold electrode
> (as well as the adhensive layer)? Will regular lift-off work?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review