Can someone suggest me a metal to use for masking GaAs/AlGaAs layers in a
Br-IBAE (Bromine,Ion beam assisted etching) machine. I tried using titanium
400angstrom layer, but that etched away. I have read in a few papers that
nickle or chromium could be used. Can some one please suggest if thats
right, I have to use HF on the sample later, so an HF resistant metal is
desired.

regards
Vaibhav Mathur
Graduate Student
University of Massachusetts,lowell
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering
Nano-Master, Inc.