Dear Prof. Yoon,

If you want to contact companies in Japan, fax them at the numbers
below.

> Shinetsu Astec                 +81-3-3293-4610
contact : Mr. Sata

> Shinetsu ......  Institute     +81-273-85-2774
contact : Mr. Katayama

> Gyodo International            +81-44-854-1979
contact : Mr. Kondo
--------------------

Sincerely,

E. H. Yang, Ph.D
Postdocoral Fellowship of JSPS
IIS, The University of Tokyo
Tel:+81-3-3402-6231(ext. 2354)
Fax:+81-3-3402-5078
email:[email protected]
URL : http://www.fujita3.iis.u-tokyo.ac.jp/~ehyang/yang.html

Jong-Hwan Yoon wrote:
>
>  I'd like to order undoped and some 3", N(100), resistivity>5 Ohm-cm,
> 200um thick silicon wafers. Please let me know how to order and make a
> payment. I hope to hear from you soon.  Thanks in advance,
>
> Best regards,
>
> Jong-Hwan Yoon
> Prof. of Physics
> Kangwon National University
> Chunchon, Kangwon-do 200-701
> KOREA
> Fax : 82-361-57-9689
> Phone : 82-361-250-8466
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Harrick Plasma, Inc.
Addison Engineering