MEMSnet Home: MEMS-Talk: how to pattern PDMS film
Nickel nanodots annealing!!
2006-10-04
madhav rao
how to pattern PDMS film
2006-10-05
Jianhua Tong
how to pattern PDMS film
Jianhua Tong
2006-10-05
Hi,everyone,

I am working on a MEMS structure and I need to pattern PDMS. the PDMS was spin
onto the wafer, the thickness is around 30 microns. I have read some papers on
PDMS pattern, but they were all made by soft lithography(use mound), this method
is difficult to form PDMS film structure.

any suggestions are welcome!

PS. Is there a kind of UV-curable PDMS available?

Thanks a lot,

Jianhua

-
Jianhua Tong
Advanced Micro&nanosystems Lab.
University of Toronto
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.