MEMSnet Home: MEMS-Talk: photoresist peeled off together with PDMS
photoresist peeled off together with PDMS
2006-10-05
Bo Bob Huo
2006-10-05
Mike Pinelis
答复: [mems-talk] photoresist peeled off together with PDMS
2006-10-05
jianshi
2006-10-05
Bill Moffat
2006-10-10
Bo Bob Huo
2006-10-11
Gareth Jenkins
AZ 9260
2006-10-11
sebastian wicklein
2006-10-13
Isaac Chan
2006-10-13
Bo Bob Huo
2006-10-13
Mike Pinelis
2006-10-14
huy vo
photoresist peeled off together with PDMS
Mike Pinelis
2006-10-05
Bob,

I have successfully used Fluid 230 from Dow Corning to solve this
problem -- it basically acts as a release layer to make sure that PDMS
does not stick to the resist.  You can spin Fluid 230 onto your
photoresist pattern and then spin or pour PDMS.

Good luck,

Mike

Mike Pinelis
Ph.D. Candidate
University of Michigan
http://www.wimserc.org
http://www.memsinvestorjournal.com




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Bo Bob Huo
Sent: Thursday, October 05, 2006 12:43 PM
To: [email protected]
Subject: [mems-talk] photoresist peeled off together with PDMS

Recently I was confused by a problem. When I peeled off PDMS from
the master coated photoresist of shipley 1818, the photoresist was
always peeled off together with PDMS. Before curing PDMS, the
master had been exposed to a vapor of the chemical of chlorinated
silane to facilitate easy removal of PDMS. Can anyone give me a
help? Thanks in advance.

-/Bob
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.
University Wafer