Hi Everyone.,

I degassed the PDMS for 1 hr using vacuum dessicator .

I immediately cured the PDMS at same 120 degree
celcius., no bubbles were found.

When I repeated the same after 30 minutes after
degassing, lot of bubbles got introduced.

Whether PDMS again absorbs the air (from atmosphere)
after degassing????

Regards

Bala.,
Mcmaster university.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
University Wafer
Addison Engineering