A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: Anyone know what this thing called and where to buyit from?
RE: Anyone know what this thing called and where to buy it from?
2006-10-20
Zhang Xuming
RE: Anyone know what this thing called and where to buyit from?
2006-10-20
Adamson, Steve
RE: Anyone know what this thing called and where to buyit from?
Adamson, Steve
2006-10-20
Guys, you need to talk with someone who is a packaging engineer. For $75
bucks you can join the International Packaging Society (IMAPS) and get a
lot of this information.=20

Ceramic packages are made by a couple of companies Kyocera and NTK,
there are probably more but they are the biggest. Coors may also be in
this game.=20

You can also by PCB packages to put die into. But these cannot be
hermetically sealed so this may not be of interest. =20


Regards,
=20
Steve Adamson
Market Manager=20
Asymtek
760-930-7274 office
760-802-1641 Cell
=20
=20

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Zhang Xuming
Sent: Thursday, October 19, 2006 8:00 PM
To: [email protected]
Subject: [mems-talk] RE: Anyone know what this thing called and where to
buyit from?

Hi Airchie:

It's called Ceramic PGA (pin grid array) package, as told by my
colleague who works on MEMS packaging.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group