Gold were elctroplating onto the edge of photoresist
2006-10-26
Michael D Martin
HV power supply
2006-10-27
Rajib Ahmed
Gold were elctroplating onto the edge of photoresist
Michael D Martin
2006-10-26
You are likely getting an enhanced deposition rate due to high field regions at
the edge of your features.  The work around for this is to do some pulse plating
with a short period of reverse bias.

-Michael Martin
 U. of Louisville


>>> "胡小东"  10/25/06 10:38 PM >>>

Dear All,
   In the past two months, while we did gold elctroplating, there were two gold
"wings" extending from the gold line onto the edge of photoresist.
   photoresist: AZ1500, 2.5 micron thick.
   gold thickness: 2 micron
   "wing" thickness: 3 to 4 micron
   "wing" width: 10 to 20 micron

   current density 5.5 mA/cm2
   electoplating time 13min
   PH value: 7
   temperature: 50 degree
   Has anyone experinced the same problem? May someone would give me any useful
suggextiongs. Thanks!

   Huxiaodong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation