MEMSnet Home: MEMS-Talk: Problem on Pt depostion by FIB
Just starting out in MEMS
2006-11-02
Jose Guevarra
2006-11-02
A.E.Reinhardt
Problem on Pt depostion by FIB
2006-11-03
jpt sharma
2006-11-05
mohendra roy
Regarding residual stress
2006-11-06
[email protected]
2006-11-06
David A. Grove
2006-11-06
Beggans Michael H IHMD
Problem on Pt depostion by FIB
jpt sharma
2006-11-03
Dear Alls
  I am having the problems to deposit Pt (making electrical contacts) using dual
beam FIB. I am using e-beam depostion (not sure why I am not using Ion beam
depostion, what I heard that ion beam may destroy the sample). Since I deposited
Pt, I was expecting the metallic behaviour when cool it down to 4.2K. But what I
get is semiconducting behaviour. Do you guys the answer? Why this happen and how
to get rid of it?
  Your reply will be highly appreciated!

  JPT
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.