MEMSnet Home: MEMS-Talk: Porous silicon: thermal expansion coefficient, specific heat
Porous silicon: thermal expansion coefficient, specific heat
2006-11-14
Miyakawa, Natsuki
2006-11-24
mohendra roy
2006-11-27
Miyakawa, Natsuki
Porous silicon: thermal expansion coefficient, specific heat
Miyakawa, Natsuki
2006-11-14
Dear all,

does anyone know the thermal expansion coefficient and specific heat of porous
silicon? I know they are strongly dependent on the porosity, so the data for
some specific parameters or rough estimation would also help.
I would appreciate any informations and suggestions from you.

Thanks a lot!

Natsuki Miyakawa

--------------------------------------------------------------------------------
---------------

Sensor Systems & Integration

EADS Deutschland GmbH
Corporate Research Centre Germany
Dept. LG-SI
81663 Munich/Germany

Phone:  +49 (0) 89.607-22875
Fax:      +49 (0) 89.607-24001
email: mailto:[email protected]
http://www.eads.net

----------------------------------------------------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.
MEMS Technology Review