MEMSnet Home: MEMS-Talk: Porous silicon: thermal expansion coefficient, specific heat
Porous silicon: thermal expansion coefficient, specific heat
2006-11-14
Miyakawa, Natsuki
2006-11-24
mohendra roy
2006-11-27
Miyakawa, Natsuki
Porous silicon: thermal expansion coefficient, specific heat
Miyakawa, Natsuki
2006-11-27
Hi,

At the moment I use the solution consisting of 9% HF + 11% H2O + 90% Isopropanol
(vol.%). Etching in the dark at the ambient temperature. P+-type, 0.02 Ohm_cm,
(100) single crystal silicon is used.
Do you happen to have the thermal properties data (TEC, specific heat) for
oxidized porous silicon (300°C in dry O2 for 1 hour)?
Thanks a lot!

Natsuki


-----Ursprüngliche Nachricht-----
Von: [email protected] [mailto:[email protected]] Im
Auftrag von mohendra roy
Gesendet: Freitag, 24. November 2006 13:46
An: General MEMS discussion
Betreff: Re: [mems-talk] Porous silicon: thermal expansion coefficient,specific
heat

first let me know in what solution you etch the silicon. Than after i can
give you the exact value of the tharmal expansion coeffcient.

On 14/11/06, Miyakawa, Natsuki  wrote:
>
> Dear all,
>
> does anyone know the thermal expansion coefficient and specific heat of
> porous silicon? I know they are strongly dependent on the porosity, so the
> data for some specific parameters or rough estimation would also help.
> I would appreciate any informations and suggestions from you.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
Mentor Graphics Corporation