MEMSnet Home: MEMS-Talk: Anisotropic Wet Etching of Silicon nitride
Anisotropic Wet Etching of Silicon nitride
2006-11-28
[email protected]
2006-11-28
[email protected]
2006-11-29
Roger Brennan
2006-11-29
[email protected]
2006-11-29
[email protected]
Ingredient of s1813 and toluene
2006-11-30
Bin Liu
2006-11-30
Roger Shile
Anisotropic Wet Etching of Silicon nitride
[email protected]
2006-11-28
Dear colleagues,

Does anybody knows a way how to ANISOTROPICALLY wet etch Silicon Nitride?

Thanks in advance for your feedback.

Cheers,
Ed S

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation