MEMSnet Home: MEMS-Talk: Anisotropic Wet Etching of Silicon nitride
Anisotropic Wet Etching of Silicon nitride
2006-11-28
[email protected]
2006-11-28
[email protected]
2006-11-29
Roger Brennan
2006-11-29
[email protected]
2006-11-29
[email protected]
Ingredient of s1813 and toluene
2006-11-30
Bin Liu
2006-11-30
Roger Shile
Anisotropic Wet Etching of Silicon nitride
[email protected]
2006-11-28
Ed:

It would be much easier to plasma etch silicon nitride anisotropically. I don't
know of a masking material that would hold up to 180 degree C. Phosphoric Acid
bath. Bob Henderson


-----Original Message-----
From: [email protected]
To: [email protected]
Sent: Tue, 28 Nov 2006 12:28 PM
Subject: [mems-talk] Anisotropic Wet Etching of Silicon nitride


Dear colleagues,

Does anybody knows a way how to ANISOTROPICALLY wet etch Silicon Nitride?

Thanks in advance for your feedback.

Cheers,
Ed S
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics