MEMSnet Home: MEMS-Talk: Parylene residue
Parylene residue
2006-11-29
rakesh babu
2006-11-29
Michael D Martin
2006-11-30
Jesse D Fowler
Parylene residue
Michael D Martin
2006-11-29
Rakesh,
   You are probably getting some sputtering of the platinum.  Turn down
your power and/or boost the pressure to reduce the kinetic energy of the
ions.

-Mike Martin
 U. of Louisville


>>> rakesh babu  11/29/2006 12:19 PM >>>
Folks,

  I was trying to etch 18um parylene using O2 plasma
with Al as the mask and after 2 hrs of etching i found
some black residue which could only be removed by
using a swab. Can anyone please tell me the reason for
this . The metal under parylene was Platinum.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
University Wafer
Harrick Plasma, Inc.