MEMSnet Home: MEMS-Talk: Quartz wet etching
Quartz wet etching
2006-12-14
Barbara Cortese
2006-12-14
[email protected]
2006-12-15
P.E.M. Kuijpers
BHF precipitates ?
2006-12-15
Andrea Mazzolari
2006-12-18
Barbara Cortese
2006-12-18
Jesse D Fowler
Quartz wet etching
[email protected]
2006-12-14
Depending upon the photoresist you probably have reflowed and filled in what was
your developed pattern with photoresist thus preventing the HF from etching the
quartz. You probably want to reduce your hard bake time after develop to what is
recommended by the resist vendor you use. They provide excellent documentation
for superior results. Bob Henderson


-----Original Message-----
From: [email protected]
To: [email protected]
Sent: Thu, 14 Dec 2006 9:10 AM
Subject: [mems-talk] Quartz wet etching


Dear all
I'm wet etching quartz with a BHF solution 6:1, but I have encounterd some
difficulties in etching.
What I do is a photolithographic process on the quartz substrate, a hardbake of
4 hours at 180° and then the wet etching process.
What I obtain though is the rearrangement of the photoresist in a disordered
pattern and no etching!
Has anyone an idea where I go wrong?
Barbara
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
________________________________________________________________________
Check out the new AOL.  Most comprehensive set of free safety and security
tools, free access to millions of high-quality videos from across the web, free
AOL Mail and more.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing