A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quartz wet etching
Quartz wet etching
2006-12-14
Barbara Cortese
2006-12-14
[email protected]
2006-12-15
P.E.M. Kuijpers
BHF precipitates ?
2006-12-15
Andrea Mazzolari
2006-12-18
Barbara Cortese
2006-12-18
Jesse D Fowler
Quartz wet etching
P.E.M. Kuijpers
2006-12-15
Dear Barbara,

Try to use a metal mask e.g. Cr.
After patterneing the Cr layer don't remove the resit befor BHF etching..

regards,
Peter Kuijpers
Philips





                                                                        To
                                       "mems-talk" 
                                                                        cc
     "Barbara Cortese"
                                               Subject
                                       [mems-talk] Quartz wet etching
     Sent by:                                               Classification
     mems-talk-bounces@me
     msnet.org

     2006-12-14 05:10 PM

      Please respond to
         General MEMS
          discussion
     






Dear all
I'm wet etching quartz with a BHF solution 6:1, but I have encounterd some
difficulties in etching.
What I do is a photolithographic process on the quartz substrate, a
hardbake of 4 hours at 180° and then the wet etching process.
What I obtain though is the rearrangement of the photoresist in a
disordered pattern and no etching!
Has anyone an idea where I go wrong?
Barbara
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
MEMStaff Inc.