2006-12-15
BOE, as opposed to just regular HF, is designed to be less aggressive
on photoresists in general.  You should be fine sticking with what
you have.  If you must change it is more important that you get a
resist that is good for the feature size and etch recepies that you
use.

Nicolas Duarte

At 1:50 PM +0100 12/15/06, Andrea Mazzolari wrote:
>Hi all, i need a photoresist resitant to boe etchants. Until now i used
>shipley s1813, it worked well, but now it is expired date.
>I'm planning to buy again shipley s1813, or is there something better ?
>
>Best regards,
>Andrea Mazzolari
>
>_______________________________________________
>Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>provider of MEMS and Nanotechnology design and fabrication services.
>Visit us at http://www.mems-exchange.org
>
>Want to advertise to this community?  See http://www.memsnet.org
>
>To unsubscribe:
>http://mail.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group