SU-8 Adhesion with SiO2
2006-12-20
Prakash Mukre
2006-12-20
Joseph Grogan
2006-12-21
John Seymour
Re: SU-8 Adhesion with SiO2
2006-12-21
Prakash Mukre
2006-12-21
John Seymour
2006-12-21
Gareth Jenkins
2006-12-21
Sueda Saylan
2006-12-21
Prakash Mukre
SU-8 Adhesion with SiO2
John Seymour
2006-12-21
Prakash, I've experienced this myself. SU-8 delamination during
development can only be solved w/ better adhesion to the underlying
layer--process params will do little to improve the situation. I
purchased a Ti oxide (http://www.siliconresources.com/AP300.html) and it
worked very well. Surface roughening or metal deposition will also work.
Good luck.
-john@MNF
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing