hi guyes,
i am having a problem.
i am doign lithography on surface, which is having 20um deep cavities. i
have to put photoresist on that.but while doing lithography the photoresist
at corner (at top surface).
i am using positive resist S1813 and spinning at speed of 3000RPM.
can anybody tell me what is the problem?
-abhay joshi
university of pune.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing