Hi all,
I am trying to fabricate a device which uses an in-plane two-arm cantilever to
rip apart a thin 100nm thick Gold bridge, which is evaporated onto the SU-8
cantilever.  This gold bridge stretches between the cantilever and another
platform also made of SU-8.

I have read that a thin film of gold (of thickness 300nm) has peak tensile
stress of 300MPa and experiences a strain of 0.05 before it breaks.  So the SU-8
cantilever needs to exert such a force on the Gold bridge to break it.

Since the gold also sits on the SU-8 and might be sheared off the SU-8 as the
cantilever moves laterally, I would like to ask whether anyone has any
information on the bond shear strength of Gold on SU-8 (I have read that the
bond pull strength of Gold on SU-8 is 4.8MPa, but I would like to know what the
bond shear strength is).



Mr. Jeffrey Mun Pun YUE
余文彬
Division of Bioengineering
Block E3, #05-18, Nanobioanalytics Lab
9 Engineering Drive 1
National University of Singapore
Singapore 117576
Tel: (65) 65165985, Fax: (65) 68723069
E-mail:  [email protected]
Website:  http://www.bioeng.nus.edu.sg/people/trau/Lab_index.htm

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer