ordered porous structure
Lung-hao Hu
2007-01-08
You wanna use the porous materials to be the dielectric layer ??
There are lots of papers talking about porous silicon. You can google it.
Also carbon nanotube is already commercialized. You purchase the bulky CNT and
then sonicate and filter out commercial CNT+surfactant to become a paper.
Or directly purchase carbon cloth to be this porous material.

Best regards,

Lung-hao Hu

Graduate Student

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
UCB 427 CO 80309 U.S.A
Email:[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.