How to clean PDMS or PLGA thin film on the Si chip
2007-01-10
欢黄
2007-01-11
Barbara Cortese
How to clean PDMS or PLGA thin film on the Si chip
Barbara Cortese
2007-01-11
You can't clean pdms with solvents but you can try dry etching (RIE) with O2!

> Hi, I have tried several ways to clean the PDMS thin film on the Silicon
> pattern(including HF, Piranha,etc). But the result is not good and
> especially I want to clean the PDMS in the hole of Si chip. Does anybody
> know how to clean it or any paper mentioned the way of cleaning?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
MEMS Technology Review
Nano-Master, Inc.