SiO2 lpcvd deposition
Andrea Mazzolari
2007-01-15
 I already deposit SiO2 at 950 C, so i don't think annealling will be
necessary.
Which LPCVD temperature do you use ?
Do you have any suggestion (gas flows) in order to obtain an high deposition
rate ?

Best regards,
Andrea.

-----Messaggio originale-----
Da: [email protected] [mailto:[email protected]] Per
conto di Qiao Dayong
Inviato: lunedì 15 gennaio 2007 5.17
A: [email protected]; [email protected]
Oggetto: Re:[mems-talk] SiO2 lpcvd deposition

3 micro SiO2 will crack due to the residual stress. My suggestion is to
deposit it three times, 1 micro each time with an annealling at 950 degree
C.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer