A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift-off Recipe
Lift-off Recipe
2007-01-15
Ravi Shankar
2007-01-16
Yue Mun Pun, Jeffrey
2007-01-16
sachin narwade
2007-01-16
Joseph Grogan
2007-01-16
Bill Moffat
2007-01-17
Yue Mun Pun, Jeffrey
Lift-off Recipe
sachin narwade
2007-01-16
Ravi Shankar,
      Lift-off is possible with S1813. You need to give a Chlorobenzene dip
on resist coated sample before UV exposure for about a minute or so
depending upon the application and the photoresist thickness you are using
(you need to standardize that). Then lift-off comes quite easily, I have
also S1813 for lift-off.

Sachin


On 1/15/07, Ravi Shankar  wrote:
>
> Hi all,
>
>    I need to use lift-off process for my device fabrication.. So far
> we haven't standardised lift-off process in our lab. We are suing
> S1813 and HNR 120 photoresists... Is it possible to achieve lift-off
> process with these low thickness photoresists? Can any one suggest
> recipe for lift-off process.. suggestions will be highly appreciated.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review