Wet etch for Titanium
2007-01-29
Yue Mun Pun, Jeffrey
2007-01-29
Barbara Cortese
Wet etch for Titanium
Barbara Cortese
2007-01-29
An etching mixture is HF(50%):H2O2(30%):H20=1:1:20..the etch rate should be 1
micrometer/min at room temperature..Have you tried a hard bake for the AZ5214E?


---------- Initial Header -----------

Date      : Mon, 29 Jan 2007 11:25:14 +0800
Subject : [mems-talk] Wet etch for Titanium

> Hi,
> I would like to know what I should use to wet etch Titanium thin films,
besides the very toxic HF?  I am looking for a combination that is friendly to
photoresists such as SU-8 and AZ5214E.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics