MEMSnet Home: MEMS-Talk: best etching for PZT
best etching for PZT
2007-01-28
Dr Nicolas Felix
2007-01-30
Hakemi, Ghazal
best etching for PZT
Hakemi, Ghazal
2007-01-30
PZT can be etched using hydrofluoric acid (HF) (+ HCl+H2O)

________________________________

From: Dr Nicolas Felix [mailto:[email protected]]
Sent: Sun 28/01/2007 22:27
To: [email protected]
Subject: [mems-talk] best etching for PZT



I'm looking for dry or wet etching of PZT piezoceramics, do you have any
idea or references for this particular topic.

Regards

Nicolas
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.