Copper plating on Aluminum seed layer
2007-02-01
Sebastian Sosin
2007-02-01
Xiaoguang "Leo" Liu
2007-02-01
IGOR KADIJA
Copper plating on Aluminum seed layer
Sebastian Sosin
2007-02-01
Does anybody have any idea (hints, published papers, experience) about
COPPER plating using an ALUMINUM seed layer or some other metal but NOT
COPPER?

Sincerely yours,

Sebastian Sosin