Dear all,

I am now trying to do PDMS to PDMS bonding. I read something about using a
liquid cushion of methanol to prevent instant boding after plasma
treatment, and thus allowing alignment of different layers. But it doesn't
work. Is there any tricks about this? My procedure is the follows,

1. drill two holes on the PDMS as the outlet for methanol evaporation.

2. Plasma treatment.

3. put the plasma treated sample in methanol for 5 mins.

3. heat in a convection oven for 80mins at 85C.

The other plasma treated samples at the same condition are all nicely
bonded without doing step 3.

Peng Li
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
Harrick Plasma, Inc.