MEMSnet Home: MEMS-Talk: PDMS to PDMS bonding
PDMS to PDMS bonding
2007-02-15
Peng Li (Paul)
2007-02-15
abdou sar
PDMS to PDMS bonding
abdou sar
2007-02-15
Hi Peng Li,
first of all without step 3 how long are you waiting to put the two PDMS slab in
contact?
As far I know the time is a big issue due to the hydrophobic recovery of the
PDMS after a O2 plasma treatment. It has been reported in different papers that
you have to put in contact the two PDMS slab within 1 min after exposure  to O2
plasma. So you should try just to put a drop of methanol between the layers and
do your alignement.

Hope that will help you!

Cheers,

Abdou
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing