Hi, I'm a graduate student at UC Berkeley. I used S1818 for high density
2um feature photolithography on Si wafer. The pattern looks great after
development with MicroDev. However, after hard bake in a 125oC oven for 30
min, the fine features turned into an area of mud/spagattii kind of mass.
Larger features, 100um lines, were still fine.

Does this mean my S1818 is bad? Or is this an intrinsic problem of S1818?
Should I reduce the hardbake temperautre and time?

Thank you!

Junyu Mai

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
Nano-Master, Inc.